[DE] Resistiver Sauerstoffsensor [EN] Exhaust gas oxygen sensor for road vehicle has oxygen sensitive-layer based on complex metal oxide including lanthanum, copper and iron |
71/73 |
Anmelder/Inhaber |
PA |
DaimlerChrysler AG, 70567 Stuttgart, DE
|
72 |
Erfinder |
IN |
Moos, Ralf, Dr., 88048 Friedrichshafen, DE
;
Rettig, Frank, 78355 Hohenfels, DE
|
22/96 |
Anmeldedatum |
AD |
24.03.2001 |
21 |
Anmeldenummer |
AN |
10114645 |
|
Anmeldeland |
AC |
DE |
|
Veröffentlichungsdatum |
PUB |
02.01.2003 |
33 31 32 |
Priorität |
PRC PRN PRD |
|
51 |
IPC-Hauptklasse |
ICM |
G01N 27/12
|
51 |
IPC-Nebenklasse |
ICS |
G01R 27/02
|
|
IPC-Zusatzklasse |
ICA |
|
|
IPC-Indexklasse |
ICI |
|
|
Gemeinsame Patentklassifikation |
CPC |
G01N 27/12
|
|
MCD-Hauptklasse |
MCM |
|
|
MCD-Nebenklasse |
MCS |
G01N 27/12
(2006.01)
|
|
MCD-Zusatzklasse |
MCA |
|
57 |
Zusammenfassung |
AB |
[DE] Die Erfindung betrifft einen resistiven Sauerstoffsensor mit einer sauerstoffsensitiven Sensorfunktionsschicht auf der Basis komplexer Metalloxide der allgemeinen Formel DOLLAR A LaCu¶1-x¶Fe¶x¶O¶3-y¶, wobei DOLLAR A La für Lanthan, DOLLAR A Cu für Kupfer, DOLLAR A Fe für Eisen, DOLLAR A O für Sauerstoff, DOLLAR A x für eine Zahl größer als ein Zehntel und kleiner oder gleich fünf Zehntel, d. h. 0,1 < x < 0,5, und DOLLAR A y für das Sauerstoffdefizit, das sich je nach Zusammensetzung aus der Elektroneutralitätsbedingung einstellt, steht. [EN] A resistive oxygen sensor has an oxygen sensitive-layer based on a complex metal oxide with the general formula LaCu1-xFexO3-y where La is Lanthanum, Cu is copper, Fe is iron, O is oxygen, and 0.1 <= x <= 0.5 and where depending upon the composition y is the oxygen deficit occurring after the establishment of electro-neutralization. No more than 10 per cent of the La ions and/or Cu ions and/or Fe ions are replaced by other ions with another valency. No more than 50 pr cent of the La ions and/or Fe ions are replaced by another ion of the same valency. The ratio of La/(Fe + Cu) in lieu 1 greater than 0.9 or less than 1.1. The oxygen sensor may incorporate a sintering agent, and an intermediate layer of SrAl2O4 between the substrate (Al2O3, MgO, ZrO2 or AIN) and the sensor functional layer. |
56 |
Entgegengehaltene Patentdokumente/Zitate, in Recherche ermittelt |
CT |
DE000002334044A DE000003723051A1 DE000003841611A1 DE000004202146A1 DE000004244723A1 DE000004325183A1 DE000004418054C1 DE000019744316A1 EP000000062994A2 EP000000191627A1 EP000000553452A2
|
56 |
Entgegengehaltene Patentdokumente/Zitate, vom Anmelder genannt |
CT |
|
56 |
Entgegengehaltene Nichtpatentliteratur/Zitate, in Recherche ermittelt |
CTNP |
|
56 |
Entgegengehaltene Nichtpatentliteratur/Zitate, vom Anmelder genannt |
CTNP |
|
|
Zitierende Dokumente |
|
Dokumente ermitteln
|
|
Sequenzprotokoll |
|
|
|
Prüfstoff-IPC |
ICP |
G01N 27/12 A11
G01R 27/02
|