[DE] Verfahren zur Herstellung von Gegenständen aus Bleikristall mit verringerter Bleilässigkeit [EN] Coating lead crystal to reduce lead loss during corrosion - by sol-gel method involving hydrolysing and condensing cpds. of silicon, aluminium, titanium or zirconium |
71/73 |
Anmelder/Inhaber |
PA |
Institut für Neue Materialien gemeinnützige GmbH, 66123 Saarbrücken, DE
|
72 |
Erfinder |
IN |
Mennig, Martin, Dr., 6607 Quierschied, DE
;
Schmidt, Helmut, Prof. Dr., 6604 Güdingen, DE
|
22/96 |
Anmeldedatum |
AD |
24.05.1991 |
21 |
Anmeldenummer |
AN |
4117041 |
|
Anmeldeland |
AC |
DE |
|
Veröffentlichungsdatum |
PUB |
26.11.1992 |
33 31 32 |
Priorität |
PRC PRN PRD |
|
51 |
IPC-Hauptklasse |
ICM |
C03C 17/25
|
51 |
IPC-Nebenklasse |
ICS |
|
|
IPC-Zusatzklasse |
ICA |
B65D 1/02
B65D 1/10
B65D 65/38
|
|
IPC-Indexklasse |
ICI |
|
|
Gemeinsame Patentklassifikation |
CPC |
C03C 17/25
C03C 2217/212
C03C 2217/213
C03C 2217/214
C03C 2217/23
C03C 2217/92
C03C 2218/113
|
|
MCD-Hauptklasse |
MCM |
|
|
MCD-Nebenklasse |
MCS |
C03C 17/25
(2006.01)
|
|
MCD-Zusatzklasse |
MCA |
|
57 |
Zusammenfassung |
AB |
[DE] Gegenstände aus Bleikristall, z. B. Karaffen und Gläser, mit verringerter Bleilässigkeit werden dadurch erhalten, daß man$A a) auf das Bleikristall eine Schutzschicht aus einer Zusammensetzung aufbringt, die nach dem Sol-Gel-Verfahren erhalten worden ist durch Hydrolyse und Kondensation von im Reaktionsmedium löslichen Verbindungen mindestens eines Elementes aus der Gruppe Si, Al, Ti und Zr, gegebenenfalls in Kombination mit im Reaktionsmedium löslichen Verbindungen mindestens eines Elementes aus der Gruppe der Alkalimetalle, Erdalkalimetalle und Bor, in einem Lösungsmittel, gegebenenfalls in Gegenwart eines Kondensationskatalysators, und$A b) die Schutzschicht wärmebehandelt. [EN] Lead crystal objects, are provided with a protective coating by the sol-gel method in which compounds of at least one element from Si, Al, Ti and Zr opt. in combination with a cpd. of at least one element from alkali metals, earth alkali metals and boron, which are all soluble in the reaction medium are hydrolysed and condensed in the presence of a condensation catalyst to produce a protective coating on the glass object. The coated object is then heat treated. USE/ADVANTAGE - Coating lead crystal carafes and glasses. The coating reduces the amount of lead escaping from the glass especially during corrosion with fluids. |
56 |
Entgegengehaltene Patentdokumente/Zitate, in Recherche ermittelt |
CT |
|
56 |
Entgegengehaltene Patentdokumente/Zitate, vom Anmelder genannt |
CT |
|
56 |
Entgegengehaltene Nichtpatentliteratur/Zitate, in Recherche ermittelt |
CTNP |
|
56 |
Entgegengehaltene Nichtpatentliteratur/Zitate, vom Anmelder genannt |
CTNP |
|
|
Zitierende Dokumente |
|
Dokumente ermitteln
|
|
Sequenzprotokoll |
|
|
|
Prüfstoff-IPC |
ICP |
B05D 7/26 O
C03C 17/25 SG
|